These zinc alloy metal name badges can easily be turned into functional pieces of art. With this matched insert charms, you can add any image, quote or photo to each charm to maximize exposure. There's a big demand in personalized gifts alike.
For sublimation or laser printer transfers.
Printing Instructions
For use in a Flat-bed press:
• Print image in reverse(mirror image)
• Tear the protective film before printing, medium pressure and image side face down;
• Printing Parameters for reference: 385 F, 45 - 55 Seconds
Remove protective film from the face of the metal.
-Before applying the transfer and metal together, dry the transfer as much as possible. This is done by laying the transfer on the top of the heating element of the press for roughly 30 seconds. Or place the transfer under an open press for 5-10 seconds. This is simply to remove as much moisture from the transfer paper as possible before making the actual transfer. Once the transfer has been dried, it should be used within a few minutes. If more than ten minutes passes before making the transfer, the transfer can be dried again prior to use.
-Using one or more paper towels, place a towel larger than the sheet of metal on the stage of the heat press.
-Next, place the metal with the transfer taped to it face down (metal is facing down, transfer facing up) on the paper towel.
-Place another paper towel(s) over the transfer and press.
-Using medium pressure, press for 45-50 seconds as needed. Do not press any longer than is needed to obtain solid rich colors, especially black. Open press and allow to cool for 10 seconds before moving. Metal remains extremely hot. Metal can be moved by handling the transfer paper or by using a spatula.
-Multiple pieces of metal can be imprinted at the same time to increase production. Be sure the entire area is sandwiched with paper towels. Do not overlap towels next to the face of the metal in that this will increase the pressure and alter color. If the image transfers correctly after pressing, but the finish of the metal plate appears mottled or hazy, lighten the pressure and/or reduce the temperature 10-15 degrees